6
what layer height is best? (forum.guncadindex.com)

is .1 or .2 layer height stronger?

you are viewing a single comment's thread
view the rest of the comments

In my experience? Doesn't really matter -- layer height influences outward print quality and dimensional accuracy more than strength.

[-] sado@fosscad.io 4 points 1 month ago

This right here. As long as your layers are bonding properly and everything else is equal, layer height is not a major factor in strength. I usually use 0.2 for most everything, and fuzzy skin to give the impression of print quality. Seems to work reasonably well:

https://i.imgur.com/OXWCyHJ.png

[-] TheShittinator@forum.guncadindex.com 4 points 1 month ago* (last edited 1 month ago)

I like to dip to 0.16 and 0.12 where it makes sense purely for quality. The mag catch on the SF5, for example, benefits from the higher resolution against high-friction surfaces and makes the paddle smoother to operate.

Print fine stuff with fine settings, more or less.

EDIT: That's a kickass-looking leber btw

[-] sado@fosscad.io 1 points 1 month ago

Thanks! It shoots great.

And yeah, if I'm doing smaller parts I'll drop the layer height down a bit on the 0.4 nozzle, or swap over to the 0.25 nozzle and drop it way down for the really small stuff. Most everything I do is large enough that I just stick to 0.4/0.2 though. Layer height around 50% of nozzle orifice seems to be a good place.