And yeah, if I'm doing smaller parts I'll drop the layer height down a bit on the 0.4 nozzle, or swap over to the 0.25 nozzle and drop it way down for the really small stuff. Most everything I do is large enough that I just stick to 0.4/0.2 though. Layer height around 50% of nozzle orifice seems to be a good place.
Thanks! It shoots great.
And yeah, if I'm doing smaller parts I'll drop the layer height down a bit on the 0.4 nozzle, or swap over to the 0.25 nozzle and drop it way down for the really small stuff. Most everything I do is large enough that I just stick to 0.4/0.2 though. Layer height around 50% of nozzle orifice seems to be a good place.