ChairManWon V3 43X in Griptape texture with Fuzzy Skin 0.1/0.1

Printed on a Qidi Q1 Pro on a 0.6 nozzle in Fiberon PPS-CF10, dried at 100C for 10hrs.

Chamber open and unheated,, bed at 80C, nozzle at 330/310C, Speed at 60mms across the board, Tree Support Organic, oriented rails up with the magwell edge flush to the plate, about 5° nose up overall.

Annealed at 127C (255F) for 16hrs.

No moisture conditioning needed.

Highest temp resistance, impervious to moisture, pretty darn stiff, rivaled in stiffness only by dry PA6-CF20.

And it goes tink-tink when you tap it, almost a metallic sound.

Yeah, I'll keep it.

Final image is a 43X in PA6-CF and the latest in PPS-CF10

this post was submitted on 12 Oct 2025
0 points (NaN% liked)

The Ark

417 readers
1 users here now

Re-upload of r/fosscad from 2015 - June 2025.

Warning: Links might be broken, images missing, etc.

Thanks to @hogleg@forum.guncadindex.com for providing the Reddit archives!

founded 6 months ago
MODERATORS